MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sekisui PIOCELAN LSP-40EB Moldable Polymer Foam
Categories: Polymer; Thermoplastic; Polyolefin; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.

Major use of Molded articles: Packing material/Returnable containers for electronic parts and Automotive parts

Information provided by Sekisui Plastic Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0250 g/cc0.000903 lb/in³After expansion; ASTM D3575
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.4469 MPa64.82 psiASTM D3575
Elongation at Break 12.1 %12.1 %ASTM D3575
Flexural Strength 0.2561 MPa37.14 psiASTM D790
Flexural Modulus 0.011847 GPa1.7183 ksiASTM D790
Compressive Strength  0.1650 MPa
@Strain 25 %
23.93 psi
@Strain 25 %
ASTM D3575
 0.2260 MPa
@Strain 50 %
32.78 psi
@Strain 50 %
ASTM D3575
 0.4630 MPa
@Strain 75 %
67.15 psi
@Strain 75 %
ASTM D3575
Compression Set 33.3 %33.3 %ASTM D3575
 
Descriptive Properties
ColorBlack
Range of center value of pre-expanded particles0.11-0.17 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sekisui PIOCELAN LSP-20DB Moldable Polymer Foam
Sekisui PIOCELAN LSP-30EB Moldable Polymer Foam
Sekisui PIOCELAN OP-30D Moldable Polymer Foam
Sekisui PIOCELAN TOPF-40DB Flame Retardant Moldable Polymer Foam
Sekisui PIOCELAN LSP-15DB Moldable Polymer Foam

PSEKIS917 / 131306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.