MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

General Industrial Polymers SBS – GP 1 Styrene/Butadiene/Styrene
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Styrene - Butadiene block copolymer designed for asphalt modification, solvent based adhesives, and for compounding applications.

Typical Polymer Composition:
Molecular Structure: Radial
Styrene Content: 30% By weight
Butadiene Content: 70% By weight
Physical Form: Pellet / Crumb

Information provided by General Industrail Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
Volatiles 0.21 %0.21 %Typical; ASTM D5668
 <= 1.0 %<= 1.0 %Range; ASTM D5668
Molecular Weight 230 - 260 g/mol230 - 260 g/molRange; ASTM D5296
 250 g/mol250 g/molTypical; ASTM D5296
Ash 0.10 %0.10 %Typical; ASTM D5667
 <= 1.0 %<= 1.0 %Range; ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 30 %30 %Typical, Bound
 29 - 33 %29 - 33 %Range, Bound
 
Descriptive Properties
Coupling EfficiencyRange, ASTM D5296
 Typical, ASTM D5296

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGENIND004 / 294793

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.