MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Intercontinental Polymers CoPET 214-02 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Applications: Low Melt

Information provided by Intercontinental Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 0.62 - 0.680.62 - 0.68Intrinsic; LCL-PR21
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
Gardner Color Number -1.00 - 4.0-1.00 - 4.0+ b; LCL-PR01
 25 - 4125 - 41Rd; LCL-PR01
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 °C410 °FLCL-PR29
Moisture Content <= 0.25 %<= 0.25 %LCL-PR08
 
Descriptive Properties
COOHMax 45 meq/kgLCL-PR09
DEG0.5 - 1.1 wt%LCL-PR11
Isophthalic Acid24 - 26 mol%LCL-PR42

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Intercontinental Polymers CoPET 159 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Intercontinental Polymers CoPET 120 CoPET Polymer Type 159 - Clear, Low Melt Polyester Pellets
Intercontinental Polymers CoPET 198 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Iran Petrochemical (PCC) PET BG-821 Polyethylene Terephthalate
Indorama AlphaPet Preformance® 1708CC(A) PET Resin

PINTER21 / 48205

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.