MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 3463V Polypropylene, Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: UV Homopolymer extrusion grade for water quench slit film. Fiber UV stability 1200 hours per ASTM G-26.

High Purity - Low catalyst residues in FINA 3463V allow extended processing runs without screen pack pluggage.

FDA - FINA 3463V complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 3463V is recommended for water quench slit films and monofilaments for carpet backing, rope, and cordage products requiring significant UV stability.

Processing - FINA 3463V processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C).

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 3.8 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 460 MPaFiber value estimated from tenacity; ASTM D3218
Modulus of Elasticity 1.515 GPaASTM D638
Tenacity 5.80 g/denierASTM D3218
Flexural Modulus 1.38 GPaFlexural modulus is 1.38 GPa. Flexural stiffness is 1.104 GPa. ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
 
Processing PropertiesOriginal ValueComments
Melt Temperature 204 - 260 °CExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6351-T6; 6351-T651
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene
Aluminum 7068-T6; 7068-T6511 Rod & Bar
Aluminum 7175-T66

PFIN60 / 38390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.