MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® H516 Polyethylene; HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: High density polyethylene compound. This high performance PE 100 HDPE compound is tailored for the demanding requirements of pressure pipe applications that require:
  • Excellent long-term hoop strength
  • Superb resistance to slow-crack growth
  • Exceptional resistance to rapid-crack propagation
  • Outstanding low-temperature toughness
Additional information: Yellow version also available.

Applications: Typical pipe applications for H516 include:

  • Gas distribution
  • Potable water
  • Industrial applications

Information provided by Phillips

This compound meets or exceeds:

  • ASTM D4976 - PE 235
  • ASTM D3350, class 445574C and 445576C
  • NSF Standards 14 and 61 for potable water
  • PPI designations PE 4710 and PE 100
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.961 g/ccASTM D-1505
Melt Flow 8.0 g/10 minHLMI, 190/21.6; ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 5000 hourslow crack growth; ASTM F-1473
Tensile Strength, Yield 25.5 MPa2 in/min, Type IV bar; ASTM D-638
Elongation at Break >= 700 %2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 0.965 GPa
@Strain 2 %
Secant; 16:1 span:depth, 0.5 in/min; ASTM D-790
Hydrostatic Design Basis 11.0 MPa
@Temperature 23.0 °C
ASTM D-2837
 
Descriptive Properties
Hydrostatic Design Basis @ 140°F MPa6.9ASTM D-2837
Hydrostatic Strength, hour >10000at 5.0MPa, 80°C; ISO 1167
 >400at 12.4Mpa, 20°C; ISO 1167
 >8000at 5.5MPa, 80°C; ISO 1167
Notched Pipe Test @ 4.6 MPa hour500ISO 13479
Rapid Crack Propagation bar>10S4 crit. pressure, -15°C; ISO 13477
 30Full Scale Test, 0°C; ISO 13478
Required Minimum Strength MPa10ISO 9080

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® H516HP High Density Polyethylene, Pressure Pipe Grade
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade
Chevron Phillips Marlex® HMN 5580 Polyethylene, Injection Molding Grade, HDPE
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer
Ineos K38-20-188 HDPE

PCHEVD239 / 20733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.