MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Panlite® L-1250Z Polycarbonate, Weather Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Injection Molding.

Applications: Electric and and electronic appliance parts, machine parts, protective equipment parts, medical equipment, lighting fixtures requiring heat resistance and trasparency; tableware and mechanical parts requiring cold and heat resistance.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.20 %23°C; 24 hr; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 77ASTM D785
Tensile Strength, Ultimate 80.0 MPaASTM D638
Tensile Strength, Yield 62.0 MPaASTM D638
Elongation at Break 140 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 2.12 GPaASTM D638
Flexural Yield Strength 92.0 MPaASTM D790
Flexural Modulus 2.23 GPaASTM D790
Compressive Yield Strength 76.0 MPaASTM D695
Izod Impact, Notched 1.40 J/cm
@Thickness 6.40 mm
ASTM D256
 8.80 J/cm
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 3.00e+16 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 60 Hz
ASTM D150
 2.95
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm
@Thickness 1.60 mm
quick pressure rise method; ASTM D149
Dissipation Factor 0.00040
@Frequency 60 Hz
ASTM D150
 0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 100 secASTM D495
Comparative Tracking Index 300 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °CASTM D648
UL RTI, Electrical 125 °C
@Thickness 1.47 mm
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.47 mm
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.47 mm
Flammability, UL94 V-2
@Thickness 1.47 mm
 V-2
@Thickness 3.05 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.585ASTM D542
Transmission, Visible 88 %
@Thickness 3.00 mm
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® ET 3113 Polycarbonate
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release
Lotte Advanced Materials Infino® SC-1060U PC Poly Optical Grade
Teijin Panlite® L-1250Z100 Transparent and Weather Resistant grade Polycarbonate Resin
Eastman Tritan™ TX1800 Copolyester

PLAT16 / 49996

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.