MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M RJS--1 3/C Phase Rejacketing System
Categories: Other Engineering Material

Material Notes: 3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of tape shield, wire shield, armored and non-armored configurations. RJS Rejacketing Assemblies are a series of silicone rubber insulator incorporating an inner expandable polyester braid designed to reduce sliding friction and deliver the insulator onto the cable. Rejacketing sleeves are designed to protect the phase legs (core) of 3/C shielded power cable from exposure to moisture, corrosion, ozone, ultra-violet radiation, physical contact and other hazards that are associated with termination operating environments. Rejacketing sleeves are designed to be used in conjunction with 3M Cold Shrink Breakout Boots and Silicone Rubber Terminations.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.650 milWall
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1058 psiASTM D412
Elongation at Break 910 %ASTM D412
50% Modulus 0.000220 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.000310 GPa
@Strain 100 %
ASTM D412
Tear Strength 32.0 kg(f)/cmASTM D624 B
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 428 kV/in
@Thickness 1.65 mm
Track Resistance 21600 secASTM D2303/IEC 587
 
Descriptive Properties
AppearanceDark Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Momentive Performance Materials Silplus™ 60 CW Heat Cured Rubber - Cable & Wire
Momentive Performance Materials Silopren™ Electro 242-0 Electrically Insulating Liquid Silicone Rubber
3M 5680 Cold Shrink Silicone Rubber Termination Kits QT-III
3M 4604 Silicone Rubber Termination Kit

PMM35231 / 169978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.