System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Celanex® MT2008 PBT, Unfilled
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.31
g/cc
1.31
g/cc
ASTM D792
Density
1.31
g/cc
0.0473
lb/in³
ISO 1183
Water Absorption
0.090 %
@Temperature 22.8 °C
0.090 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow
0.018
-
0.020
cm/cm
0.018
-
0.020
in/in
ASTM D955
0.018
-
0.020
cm/cm
0.018
-
0.020
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
72
72
ISO 2039-2
Tensile Strength at Break
60.0
MPa
8700
psi
5mm/min; ISO 527-2/1A
Tensile Strength, Yield
55.2
MPa
8000
psi
ASTM D638
Elongation at Break
5.0 %
5.0 %
5mm/min; ISO 527-2/1A
5.0 %
5.0 %
ASTM D638
Flexural Strength
80.0
MPa
11600
psi
ISO 178
82.7
MPa
12000
psi
ASTM D790
Flexural Modulus
2.20
GPa
319
ksi
ISO 178
2.28
GPa
330
ksi
ASTM D790
Izod Impact, Notched
0.267
J/cm
0.500
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
3.10
kJ/m²
1.48
ft-lb/in²
ISO 180/1A
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
IEC 60093
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
ASTM D150
3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
15.0
kV/mm
381
kV/in
IEC 60243-1
15.7
kV/mm
400
kV/in
short term; ASTM D149
Dissipation Factor
0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Thermal Properties
Metric
English
Comments
Melting Point
225
°C
437
°F
10°C/min; ISO 11357-1,-2,-3
225
°C
437
°F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
154
°C
310
°F
ASTM D648
155
°C
311
°F
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
54.4
°C
130
°F
ASTM D648
57.0
°C
135
°F
ISO 75-1, -2
Glass Transition Temp, Tg
60.0
°C
140
°F
ISO 11357-1,-2,-3
Flammability, UL94
HB
HB
Processing Properties
Metric
English
Comments
Processing Temperature
65.0
-
93.0
°C
149
-
199
°F
cavity
250
-
260
°C
482
-
500
°F
hot runner
Feed Temperature
230
-
240
°C
446
-
464
°F
Zone 1
230
-
240
°C
446
-
464
°F
Zone 2
235
-
250
°C
455
-
482
°F
Zone 3
235
-
250
°C
455
-
482
°F
Zone 4
240
-
260
°C
464
-
500
°F
Die Temperature
250
-
260
°C
482
-
500
°F
Melt Temperature
243
°C
469
°F
ISO 294
235
-
260
°C
455
-
500
°F
Mold Temperature
82.0
°C
180
°F
ISO 294
Injection Velocity
300
mm/sec
11.8
in/sec
ISO 294
Drying Temperature
120
-
130
°C
248
-
266
°F
Dry Time
4.00
hour
4.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Hold Pressure
48.0
MPa
6960
psi
ISO 294
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Processing conditions acc. ISO
7792-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celanex® 2401 MT PBT, Medical Technology
Celanese Celanex® 2300 GV1/10 PBT, 10% Glass Reinforced
Celanese Celanex® 2008 PBT, Unfilled
Celanese Celanex® 2003HR PBT, Unfilled
Celanese Celanex® 2002-3 PBT, Unfilled
PHCQ093 / 178548
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.