MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Heat-Away™ 639 Thermally Conductive Grease, Aluminum Filled
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: Aremco's Heat-Away™ thermal greases are ceramic and metal-filled silicone systems which offer exceptional thermal and electrical properties to 550 ºF. These materials are used in high-power electronic devices, heat pipes, and other heat exchange systems.

Vendors: Aremco's Heat-Away™ greases are ceramic and metalfilled systems that offer exceptional electrical and thermal properties. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
Solids Content 100 %
Water Absorption 0.00 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10000 ohm-cm
Dielectric Strength 40.0 V/milExposure to voltages in excess of rated maximum can cause permanent electrical leak paths
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 21.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 550 °F
Minimum Service Temperature, Air -60.0 °F
 
Descriptive Properties
Chemical ResistanceExcellent
ColorAluminum
FillerAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Heat-Away™ 640 Thermally Conductive Grease, Copper Filled
Aremco Heat-Away™ 641 Thermally Conductive Grease, Silver Filled
Lord Adhesives Gelease™ MG-100 Thermally Conductive Silicone Gel Interface
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2

PAREM28 / 24292

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.