MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds Body Double™ SILK Silicone rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Body Double™ SILK is a self-releasing platinum-cure silicone rubber that can be applied directly to the skin to make molds of the face, hands and other body parts. The rubber cures quickly and will reproduce excellent detail from any original model. Certified Skin Safe - Material is skin safe and certified by an independent laboratory. Body Double™ SILK will release from closely cropped hair-covered skin surfaces (short beards, moustaches, eye-brows, pubic hair, etc.). Release cream or Hyperfolic™ are not needed when using Body Double™ SILK. Body Double™ SILK will last for many castings of almost any material including plaster, Matrix™ Neo™, wax, resins (Smooth-Cast urethanes, polyester, etc.) Body Double™ SILK has a working time of 6 minutes and a demold time of 20 minutes*.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM D-2240
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 minWorking
 20.0 minDemold
Pot Life 6.00 minASTM D-2471
 
Descriptive Properties
ColorGreen
Mix Ratio1A:1Bby weight
Mixed ViscosityBrushable
Specific Volume30.4[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN315 / 297016

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.