MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC NORYL™ Resin FNH2160 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ FNH2160 resin is a foamable blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS) and offers 20% weight reduction at 6.35mm (0.250”) wall. This material contains non-brominated, non-chlorinated flame retardant with a UL94 flame rating of 5VA at 3.9 mm and V1 at 3mm. NORYL FNH2160 resin offers fast cycle time, improved processing, and exhibits good dimensional stability and low moisture absorption. The unique combination of properties in this structural foam material allows for designing optimum wall thickness in computer and business machine applications, electrical enclosures/housings, medical equipment, and hospital bed rails and components.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccfoam molded; ASTM D792
 1.12 g/cc1.12 g/ccASTM D792
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
ASTM D570
Viscosity 36 cP
@Load 5.00 kg,
Temperature 280 °C
36 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 6.40 mm
0.0050 - 0.0080 in/in
@Thickness 0.252 in
SABIC method
 
Chemical PropertiesMetricEnglishComments
Blowing Agent Content 1.0 - 3.0 %1.0 - 3.0 %
 2.0 %2.0 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.0 MPa
@Thickness 6.35 mm
4930 psi
@Thickness 0.250 in
ASTM D638
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ASTM D638
 36.0 MPa
@Thickness 6.35 mm
5220 psi
@Thickness 0.250 in
ASTM D638
Elongation at Break 12 %
@Thickness 6.35 mm
12 %
@Thickness 0.250 in
ASTM D638
Elongation at Yield 3.04 %3.04 %50 mm/min; ASTM D638
Tensile Modulus 2.68 GPa389 ksi50 mm/min; ASTM D638
Flexural Strength 70.0 MPa
@Thickness 6.40 mm
10200 psi
@Thickness 0.252 in
yield; ASTM D790
Flexural Modulus 2.25 GPa
@Thickness 6.40 mm
326 ksi
@Thickness 0.252 in
ASTM D790
Izod Impact, Unnotched 3.62 J/cm
@Thickness 6.40 mm
6.78 ft-lb/in
@Thickness 0.252 in
ASTM D4812
Dart Drop, Total Energy 29.0 J21.4 ft-lbpeak; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 6.40 mm
199 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
@Thickness 6.40 mm
180 °F
@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94  V-1
@Thickness >=3.00 mm
V-1
@Thickness >=0.118 in
UL 94
 V-0
@Thickness >=6.00 mm
V-0
@Thickness >=0.236 in
UL 94
 5VA
@Thickness >=3.90 mm
5VA
@Thickness >=0.154 in
UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 260 °C446 - 500 °F
Middle Barrel Temperature 270 - 305 °C518 - 581 °F
Front Barrel Temperature 270 - 305 °C518 - 581 °F
Nozzle Temperature 270 - 305 °C518 - 581 °F
Melt Temperature 270 - 310 °C518 - 590 °FStructural Foam Molding
Mold Temperature 25.0 - 55.0 °C77.0 - 131 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °FStructural Foam Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourResin; Structural Foam Molding
 8.00 hour8.00 hourResin, Cumulative; Structural Foam Molding
 
Descriptive Properties
Blowing Agent, Physical SystemNitrogen Gas
FOAM - Flame Class Minimum Density0.85 g/cm³
FOAM - IMPACT 6.4 mm Wt Reduction20 %
FOAM - MECHANICAL 6.4 mm Wt Reduction20 %
FOAM - PHYSICAL 6.4mm Wt Reduction20 %
FOAM - THERMAL 6.4mm Wt Reduction20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82299 / 290246

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.