MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow LDPE 683I Low Density Polyethylene, Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/cc
Melt Flow 0.70 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.3 MPa
Film Tensile Strength at Yield, TD 10.3 MPa
Film Elongation at Break, MD 360 %
Film Elongation at Break, TD 530 %
Coefficient of Friction 0.50
Elmendorf Tear Strength MD 270 gUnspecified film thickness
Elmendorf Tear Strength TD 290 gUnspecified film thickness
Dart Drop Test 140 g
Film Tensile Strength at Break, MD 27.6 MPa
Film Tensile Strength at Break, TD 19.3 MPa
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
Gloss 64 %45°
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LDPE 955I Low Density Polyethylene
Dow LDPE 493A Low Density Polyethylene, Film Grade
Dow LDPE 510I Low Density Polyethylene
Dow LDPE 640IM Low Density Polyethylene
Dow LDPE 722M Low Density Polyethylene

PDW512 / 34581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.