MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.

Clarity. M6823MZ incorporates the latest generation of clarification technology resulting in excellent cycle time and superior performances in thin-wall, multi-cavity molds.

FDA. M6823MZ complies with FDA regulations Title 21 CFR Section 177.1520 (c) 3.1 and may be used under these provisions for food contact and packaging.

Recommended Applications. M6823MZ is a medium molecular weight material recommended for injection molding. However, due to its unique and interesting properties, other applications may exist.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 30 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 29.0 MPaASTM D638
Elongation at Yield 12 %ASTM D638
Tensile Modulus 1240 MPaASTM D638
Flexural Modulus 1190 MPaASTM D790
Izod Impact, Notched 37.0 J/mASTM D256
Impact Test 12.2 ft-lb
@Thickness 3.17 mm
Drop Impact; API
 
Thermal PropertiesOriginal ValueComments
Melting Point 136 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %
@Thickness 1.02 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 - 480 °F
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total 6823MZ Polypropylene, Injection Molding Grade
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion
BASF Novolen® 3520 L Polypropylene
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene

PTOTAL869 / 130594

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.