MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Matexcel CER-0110 HAP (Spherical) Powder, 200nm
Categories: Ceramic

Material Notes: Hydroxyapatite, also called hydroxylapatite (HA), is a naturally occurring mineral form of calcium apatite. It makes up most of the human bone structure, builds tooth enamel, and collects in tiny amounts in part of the brain.

HAP; Hydroxyapatite; CER-0008; HAP (Spherical) Powder, 12-100µm; HAP Spherical; food grade HAP; toothpaste; mouthwash

Application: Toothpaste additive or mouthwash product

Morphology: White powder

Uses: Generally 1-5wt% addition of final product.

Key Words: Synonyms: HAP; Hydroxyapatite; Source: Synthesis
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.20 µm0.20 µm
Storage Temperature 20.0 °C68.0 °F
 
Descriptive Properties
CAS Number12167-74-7
Product overviewThis product is manufactured by chemical synthesis. This product is food grade and suitable be used in toothpaste additive or mouthwash product.
Purity>96%
Shipping & PackagingAluminum foil bag packaging

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1548 / 300179

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.