MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 960.5 Polysulfone (PSU), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D 792
Additive Loading 5.0 %5.0 %Primary Additive
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 74.5 MPa10800 psiASTM D 638
Elongation at Break 5.0 %5.0 %ASTM D 638
Tensile Modulus 2.76 GPa400 ksiASTM D 638
Flexural Strength 123 MPa17800 psiASTM D 790
Flexural Modulus 3.10 GPa450 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 11.2 J/cm
@Thickness 3.20 mm
21.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmASTM D 257
Surface Resistance <= 10000 ohm<= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  37 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
37 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 38 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
38 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 38 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
38 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 39 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
39 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 40 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
40 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 49 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
49 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 177 °C350 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 332 - 357 °C630 - 675 °F
Mold Temperature 93.3 - 149 °C200 - 300 °F
Drying Temperature 135 °C
@Time 14400 sec
275 °F
@Time 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 961 Polysulfone (PSU), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company RTP 983 Polysulfone (PSU), Carbon Fiber
RTP Company RTP 299 X 131299 A Nylon 6/6 (PA), Carbon Fiber - Glass Fiber - Impact Modified - Heat Stabilized - Electrically Conductive - Preliminary Datasheet
RTP Company ESD C 901 Polysulfone (PSU), Glass Fiber - ESD Protection - Electrically Conductive
RTP Company ESD C 105 Polypropylene (PP), Glass Fiber - ESD Protection - Electrically Conductive

PQZWA678 / 92169

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.