MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® 9415(Z) Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Medium viscosity, flame retardant extrusion and injection molding grade with 10% standard glass fibers and easy mold release agent.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/cc
Moisture Absorption at Equilibrium 0.12 %50% RH
Water Absorption at Saturation 0.29 %
 0.29 %
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmASTM D955
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75ASTM D785
Tensile Strength, Ultimate 69.0 MPaASTM D638
Tensile Strength, Yield 80.0 MPaASTM D638
Elongation at Break 10 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Tensile Modulus 4.00 GPa
Flexural Yield Strength 103 MPaat 5% strain; ASTM D790
Flexural Modulus 3.40 GPaASTM D790
Izod Impact, Notched 1.10 J/cm
@Thickness 3.20 mm
ASTM D256
Charpy Impact Unnotched 10.0 J/cm²
Tensile Creep Modulus, 1 hour 5900 MPa
Tensile Creep Modulus, 1000 hours 5400 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
 3.2
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
Dissipation Factor 0.00090
@Frequency 100 Hz
 0.0080
@Frequency 1e+6 Hz
Arc Resistance 115 secTungsten Electrodes; ASTM D495
Comparative Tracking Index 175 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 38.0 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.13 J/g-°CASTM D2766
Thermal Conductivity 0.210 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
Vicat Softening Point 144 °C
Glass Transition Temp, Tg 148 °C
UL RTI, Electrical 125 °C
UL RTI, Mechanical with Impact 115 °C
UL RTI, Mechanical without Impact 125 °C
Flammability, UL94 V-0
@Thickness 1.60 mm
Oxygen Index 35 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
Covestro Makrolon® 9425 Polycarbonate
INEOS Styrolution Luran® S KR 2861/1 C Colored ASA+PC
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
INEOS Styrolution Luran® S KR 2867 C WU Colored ASA+PC

PBA455 / 26956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.