MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Retelan® NFV0 Flame Retardant ABS compound
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes:

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ASTM D792
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
0.30 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inSO.F.TER Method
Melt Flow 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
32 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 40.0 MPa5800 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 2.10 GPa305 ksiASTM D638
Flexural Strength 60.0 MPa8700 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 1.10 J/cm2.06 ft-lb/inASTM D256/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
Dielectric Constant 3.13.1ASTM D150
Dielectric Strength 32.0 kV/mm
@Thickness 1.60 mm
813 kV/in
@Thickness 0.0630 in
ASTM D149
Dissipation Factor 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FASTM D648
Vicat Softening Point 85.0 °C185 °F120°C/h at 50 N; ASTM D1525
 95.0 °C203 °F120°C/h at 10 N; ASTM D1525
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 601 FR Acrylonitrile Butadiene Styrene (ABS), Glass Fiber - Flame Retardant - UL94 V-0
LG Chemical AF-348 ABS, Flame Retardant, Heat Resistant, Weather Resistant
RTP Company RTP 603 FR Acrylonitrile Butadiene Styrene (ABS), Glass Fiber - Flame Retardant
Akro-Plastic Akromid® A3 K1 FR natural (2312) PA 6.6 Dry, 25% Glass Filled, Flame Retardant
RTP Company RTP 605 FR  Acrylonitrile Butadiene Styrene (ABS) Glass Fiber 30% - Flame Retardant

PSOFS953 / 162417

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.