MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Selenis ECO INFINITE 001 Recycled Copolyester for Packaging
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis ECO INFINITE 001 is a PET copolymer resin, suitable for stretch blow molding in one or two stages and extrusion processes, with up to 50% post-consumer RPET, a packaging solution that will fit the expectation of brand owners looking to maximize sustainability. Selenis ECO INFINITE 001 is the answer for those looking to maintain packaging aesthetics and complete functionality of processing, whilst providing a more eco-friendly alternative. Selenis quality inspection practices allow us to control the physical properties and consistently provide the deliverables required by customers. Selenis ECO INFINITE 001 is especially recommended for general applications, which the main requirements are the balance of optical and mechanical properties. It is particular suitable for bottles, film applications and general-purpose packages.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium <= 0.20 %
Viscosity Test 80 - 84 cm³/gIntrinsic; ISO 1628-5
Crystallinity >= 50 %ASTM D1505
ASTM Color <= 5.0b*; ASTM D6290
 >= 68L*; ASTM D6290
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 1.00 ppmASTM F2013
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 255 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °C
Drying Temperature 175 °C
@Time >=14400 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE963 / 243462

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.