MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KLJ Group Kanatol 900 Plasticizer
Categories: Fluid

Material Notes: Properties: DINP is almost colourless and odorless oily liquid, free of foreign materials which is slightly soluble in water ( 0.285mg/L at 24°C ) but soluble in alcohols, hexane etc. It is miscible and compatible with all the monomeric plasticizers of PVC compounding.

Application: Around 95% of DINP is used in PVC as a plasticizer. More than half of the remaining 5% is used in the production of polymers other than PVC (e.g. rubbers). The remaining DINP used in non-polymer application including anticorrosion paints, anti-fouling paints, lacquers, inks, adhesives and sealants. DINP is a monomeric primary plasticizers of medium molecular weight and fine performance. It has been developed to fulfill the need for an economical plasticizer in formulation which require very low volatility and good permanence characteristics. This products is widely used in vinylic compounds including wires, cables and plastisols.

Chemical Name: DINP

Molecular Formula: C 26 H42 O4

Molecular Structure: 26 H42 O4

CAS Number: 28553-12-0

EINECS NO.: 249-079-5

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 - 0.976 g/cc
@Temperature 27.0 °C
ASTM D1045-08
Viscosity 76 - 82 cPKLJ TM-P-13-97
Molecular Weight 418 g/mol
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.30e+11 - 2.70e+11 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Boiling Point 250 °C
@Pressure 0.000700 MPa
Pour Point -48.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.483 - 1.489
@Temperature 27.0 °C
ASTM D1045-08
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM D1045-08
Shelf Life 24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.03%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.01%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<20Hazen, ASTM D1045-08
Content<0.1%Residual/Free Alcohol, KLJ TM-P-12-98
 >99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 264-270 mg KOH/gmEster Value, ASTM D1045-08
Volatile Loss<0.1%130°C for 3 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ166 / 284187

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.