MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Johnson Matthey B Bronze™ Copper Based Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: JM Bronze™ filler metals are a range of special products designed for high temperature brazing of steel and carbide components. These products contain nickel and or manganese and show improved wetting on tungsten carbide.

B Bronze™ was developed for furnace brazing of stainless steel under reducing atmospheres. The joints produced in both ferritic and austenitic steels exhibit resistance to interfacial corrosion. It will penetrate joint gaps ranging from an interference fit up to 0.5 mm and has consequently been used to braze mild steels where the gaps are too large for copper (i.e. over 0.025 mm).

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 1081 - 1101 °C1978 - 2014 °F
Solidus 1081 °C1978 °F
Liquidus 1101 °C2014 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.030 %0.030 %
Copper, Cu 97 %97 %
Nickel, Ni 3.0 %3.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey C Bronze™ Copper Based Brazing Filler Metal
Johnson Matthey F Bronze High Temperature Alloy for Tungsten Carbide Brazing
Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing
Overview of materials for Solder/Braze Alloy
Johnson Matthey J Bronze™ Copper Based Brazing Filler Metal

NJMMJ9869 / 186270

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.