Notes: Telcar OBC 1383N is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Telcar OBC 1383N is a medium hardness grade suitable for injection molding and extrusion. Features: Filled; Low Density; Low Flow; Medium Hardness Uses: General Purpose; Industrial Applications; Weatherstripping Form: Pellets Processing Method: Extrusion; Injection Molding Information Provided by Teknor Apex |