Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features:- High flexibility and toughness
- Good thermoforming and orientation properties
- High shrinkage
- Good transparency
- Low melting point (200°C)
Application examples: Grilon CR 9 is suitable for the manufacture of both blown and cast coextruded film. Grilon CR 9 is suitable for the following applications: Flexible packaging, e.g. “Cook in ham”, consumer packaging of meat, cheese, smoked ham, fish, sausage, poultry and peanuts as well as many other foodstuffs.Information provided by EMS Grivory. |