MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Lacovyl® EF 821 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: LACOVYL EF 821 is a very high molecular weight vinyl chloride homopolymer manufactured by emulsion polymerization process for the preparation of plastisols.

Its is particularly suitable for the manufacture of rigid foams and compact articles where excellent mechanical properties are required.

* MAIN CHARACTERISTICS

Viscosity index (ISO 1628-2):200 ml/g,(K value:86).

* APPLICATIONS

LACOVYL EF 821 is suitable for use in the following applications:

  • transparent surface layer,
  • compact layer to increase resistance to abrasion,
  • blended with other resins in flexible foams to improve resilience,
  • in rigid foams for insulation or to reduce the weight of the structures.

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Number 200 cm³/g
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. reports 'Transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Lacovyl® EF 701 PVC
Arkema Lacovyl® BB 9010 PVC
Overview of materials for PVC, Molded
Arkema Lacovyl® GA 7701 Vinyl Copolymer
Arkema Lacovyl® GA 7701 H Vinyl Copolymer

PZARKG268 / 25564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.