Description: NBR 6840 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6840 is a non staining, medium low mooney, and medium high acrylonitrile polymer designed for easy processing, high productivity and excellent elastic properties. NBR 6840 offers very low mold fouling, fast cure, and high resilience. Applications: NBR 6840 is recommended to use in wide range of general purpose applications including injection molded o-rings, calendared belting, extruded hose and sponge. CAS No: 9003-18-3 Information provided by LG Chemical |