MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: HDPE HMW 1000950 features good melt strength, excellent stress cracking resistance, good rigidity, and excellent impact strength. Applications include agricultural chemical tanks, pallets, and large formed and blow molded parts.

Former A-Top Polymers product; part of Amco product line since 2013.

Key Words: FDA 21CFR177.1520
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D1505
ESCR 100% Igepal® >= 600 hourCondition A, F50
 >= 600 hourCondition B, F50
Melt Index of Compound 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3600 psi50 mm/min, Type IV; ASTM D638
Elongation at Break >= 600 %50 mm/min, Type IV; ASTM D638
Flexural Modulus 170 ksiASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -131 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beijing Evergrow Resources UHF-R2400 UHMW PE Fiber
BASF Elastollan® S 50 A SPF TPUR
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
ExxonMobil HPA 020 Molding High Density Polyethylene (HMW) Resin
ExxonMobil HTA 001HD High Density Polyethylene (HMW) Resin

PATOP014 / 79957

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.