System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
ExxonMobil Exxsol™ D40 Dearomatized Fluid
Categories:
Fluid
Material Notes:
Availability: Africa & Middle East, Asia Pacific, Europe, North America and South America
Appearance: Clear/Transparent Liquid
Information provided by ExxonMobil
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
6.47
lb/gal
@Temperature 15.0 °C
ASTM D4052
Kinematic Viscosity
1.28
cSt
ASTM D445
Vapor Pressure
<=
1.00
torr
@Temperature 20.0 °C
ExxonMobil Method
Thermal Properties
Original Value
Comments
Boiling Point
325
°F
Initial; ASTM D86
Flash Point
113
°F
ASTM D93
Descriptive Properties
Aniline Point
156°F
Method E, ASTM D611
Aromatic Content
<0.1%
UV, ExxonMobil Method
Dry Point
369°F
ASTM D86
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
ExxonMobil Exxsol™ D60 Dearomatized Fluid
ExxonMobil Exxsol™ D80 Dearomatized Fluid
PEX99590 / 175826
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.