MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Go Yen Chemical GYM-1000 GYC Senior Mica Powder Sericite
Categories: Other Engineering Material

Material Notes: GYM-1000 have a smooth surface, high reflectivity, excellent adhesion, chemical resistance, heat resistance, good process-ability and dispersion, low thermal expansion coefficient, good insulation, toughness and high resistance. Especially suitable for plastic extruding and injection, mixing and calendaring. In addition can also be as excellent rubber release agent, mold, sticking prevention agent, anti adhesion agent.

Applications:

  • Rubber
  • Plastic
  • Insulation
  • Heat insulation
  • Paint
  • Ceramic
  • Electrode
  • Petroleum
  • Borehole

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 - 2.85 g/cc0.101 - 0.103 lb/inĀ³
Particle Mesh Size <= 325 Mesh<= 325 Mesh0.99
pH 7.0 - 9.07.0 - 9.0
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.50 - 1.601.50 - 1.60
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %105?
 
Descriptive Properties
AppearancePowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN857 / 267165

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.