MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond F253 Color Keyed High Temperature Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mixture is green/blue; and the fully cured adhesive is reddish-amber. It exhibits excellent wicking, and develops strong, tough mechanically stable bonds to a wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics. In addition, TRA-BOND F253 has good impact and thermal shock resistance, demonstrates low stress, and yields excellent pot and polish connections. It is also resistant to water and weathering, vapors and gases, most petroleum products, and an extended range of organic and inorganic environments. An additional post-cure of 30 minutes at 150°C is recommended when application temperatures higher than 150°C are anticipated.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccMixed
Solids Content 100 %Reactive Solids Content
Volatile Organic Compounds (VOC) Content 19.6 g/l
Water Absorption 0.0040 %After 24 hours
Viscosity 1750 cP
@Temperature 25.0 °C
Mixed (sp #2, 6 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Adhesive Bond Strength 2700 psiLap shear, alum to alum
 
Thermal PropertiesOriginal ValueComments
CTE, linear 62.7 µm/m-°CBelow Tg
 202 µm/m-°CAbove Tg
Maximum Service Temperature, Air 175 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 116 °CUltimate Tg
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.56
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Temperature 150 °C
 5.00 min
@Temperature 125 °C
 15.0 min
@Temperature 100 °C
Pot Life 60 min25 grams
 
Descriptive Properties
Color Green BlueMixed
 Light YellowUnmixed
 Reddish-AmberCured
Mix Ratio, parts by weight100/10Resin/Hardener
Working Life hours 225 grams

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F253M Color Keyed High Temperature Epoxy Adhesive
Tra-Con Tra-Bond F253HV Color Keyed High Temperature Epoxy Adhesive
Atom Adhesives AA-BOND F253 Epoxy Adhesive

PTRAC250 / 71178

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.