MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sika SikaQuick® 100 Rapid hardening repair mortar with extended working time
Categories: Other Engineering Material

Material Notes: SikaQuick® 1000 is a 1-component, rapid hardening, early strength gaining, cementitious, patching material for concrete.

Where to Use:

  • Use on grade, above, and below grade on concrete.
  • Highway overlays and repairs.
  • Structural repair material for concrete roadways, parking structures, bridges, dams and ramps.
  • Full depth patching repairs.
  • Economical patching material for horizontal repairs of concrete and mortar.
Advantages:
  • Specially suited for hot weather applications when extended working time is required.
  • Rapid hardening as defined by ASTM C-928.
  • Epoxy coatings can be applied as early as 6 hrs. On site testing is recommended for verification.
  • Freeze/thaw resistant.
  • Easy to use, labor-saving material.
  • Not gypsum-based.
  • High early strength.
  • Open to foot traffic in 4 hours; to vehicle traffic in 6 hours (at 73°F).
  • Easily applied to clean, sound substrate.
  • Not a vapor barrier.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  2.07 MPa
@Time 86400 sec
300 psi
@Time 24.0 hour
Splitting; ASTM C496
 2.07 MPa
@Time 2.42e+6 sec
300 psi
@Time 672 hour
Direct Tensile, substrate failure; ACI 503
 2.76 MPa
@Time 605000 sec
400 psi
@Time 168 hour
Splitting; ASTM C496
 3.45 MPa
@Time 2.42e+6 sec
500 psi
@Time 672 hour
Splitting; ASTM C496
Modulus of Elasticity 31.7 GPa4600 ksiASTM C-469
Flexural Strength  4.83 MPa
@Time 86400 sec
700 psi
@Time 24.0 hour
ASTM C78
 6.21 MPa
@Time 605000 sec
900 psi
@Time 168 hour
ASTM C78
 6.89 MPa
@Time 2.42e+6 sec
1000 psi
@Time 672 hour
ASTM C78
Compressive Strength  8.62 MPa
@Time 10800 sec
1250 psi
@Time 3.00 hour
Mortar; ASTM C-109
 27.6 MPa
@Time 86400 sec
4000 psi
@Time 24.0 hour
Mortar; ASTM C-109
 34.5 MPa
@Time 605000 sec
5000 psi
@Time 168 hour
Mortar; ASTM C-109
 48.3 MPa
@Time 2.42e+6 sec
7000 psi
@Time 672 hour
Mortar; ASTM C-109
Adhesive Bond Strength  2.07 MPa
@Time 2.42e+6 sec
300 psi
@Time 672 hour
Direct Tensile Bond; ACI 503
 12.1 MPa
@Time 86400 sec
1750 psi
@Time 24.0 hour
ASTM C882
 13.8 MPa
@Time 605000 sec
2000 psi
@Time 168 hour
ASTM C882
 17.2 MPa
@Time 2.42e+6 sec
2500 psi
@Time 672 hour
ASTM C882
Abrasion 0.026
@Time 2.42e+6 sec
0.026
@Time 672 hour
Resistance, Inches of Wear at 1 hr.; ASTM C779
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.060 %0.060 %Drying; ASTM C596
 
Processing PropertiesMetricEnglishComments
Cure Time 40.0 - 90.0 min0.667 - 1.50 hourInitial Set; ASTM C266
 60.0 - 120 min1.00 - 2.00 hourFinal Set; ASTM C266
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
12.0 Month
@Temperature 39.2 - 95.0 °F
in original unopened cartridge
 
Descriptive Properties
ColorConcrete gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIKA944 / 209851

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.