MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M low brazing temperature and narrow solidus, liquidus range makes it ideal for applications where temperature is a factor with slow heating rates, such as in furnace brazing.

Applications:

Silvaloy 18M is used for joining copper and copper alloys, such as brass or bronze. It is suitable for use on silver, tungsten, and molybdenum. It should not be used on ferrous nickel alloys. On copper to copper applications, it is self-fluxing due to the fluxing action of the phosphorus content. It's low melting temperature makes it ideal for application on copper to brass temperature and dezincification is a factor.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 8.35 g/cc
Density 0.302 lb/in³
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000290 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1190 - 1235 °F
Solidus 1190 °F
Liquidus 1235 °F
Maximum Service Temperature, Air 400 °Fcontinuous
 500 °Fintermittent
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1225 - 1350 °FBrazing Temperature
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 74.35 - 77 %As balance
Other, total <= 0.15 %
Phosphorus, P 6.0 - 6.5 %
Silver, Ag 17 - 19 %
 
Descriptive Properties
ColorLight Copper
Electrical Conductivity (% IACS)6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reade Advanced Materials Iron Chromite (FeO·Cr2O3)
Elmet-Starck Pure Niobium (Columbium)
Chromium Nitride (CrN) PVD Coating
Boron, B
Tungsten, W

NBRW017 / 79793

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.