- Developmental product
- (PC+PBT)-blend
- impact modified
- easy release
- UV-stabilized
- injection molding grade
Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flowability beside excellent chemical resistance.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |