MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CENTROPLAST CENTROPEEK Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medical equipment.

Information provided by CENTROPLAST Engineering Plastics GMBH

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.45 %in water at 23°C; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105
@Thickness 10.0 mm
ISO 2039-2
Ball Indentation Hardness 230 MPavalue at 30 sec.; ISO 2039-1
Tensile Strength, Yield 110 MPav = 50 mm/min; ISO 527-2
Elongation at Break 20 %ISO 527-2
Tensile Modulus 4.40 GPaISO 527-2
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 100 Hz
IEC 60250
 3.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mmin transformer oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 60250
 0.0020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359
Thermal Conductivity 0.250 W/m-K
Melting Point 340 °C10K/min; ISO 3146
Maximum Service Temperature, Air 250 °CLong Term
 310 °CShort term
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75-2
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 6.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron™ LSG PEEK Extruded Unfilled Polyetherether Ketone
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Akro-Plastic Akrotek® PEEK natural (5184) PEEK, Dry
Overview of materials for Polyetheretherketone, PTFE Filled

PCENTR24 / 27975

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.