MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-16120G Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-16120 G XRD1 is a high performance thermoplastic elastomer specifically designed for healthcare and medical applications. Medalist MD-13240 is a low hardness, low density, halogen-free grade that can be sterilized and is suitable for cast film extrusion, and injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Colorability; Good Moldability; Good Processability; Good Sterilizability; Halogen Free; High Elongation; High Flow; Low Density; Low Hardness; Lubricated; Soft

Uses: Disposable Hospital Goods; Medical/Healthcare Applications; Pharmaceuticals; Prosthetics; Rubber Replacement; Soft Touch Applications

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data.

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.842 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 0.325 kg,
Temperature 125 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 20
@Time 5.00 sec
Injeciton Molded; ASTM D2240
 23
@Time 1.00 sec
Injeciton Molded; ASTM D2240
Tensile Strength at Break 200 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain 5.08 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 6.38 psi
@Strain 200 %
Die C, 20 in/min; ASTM D412
 7.83 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 1300 %Die C, 20 in/min; ASTM D412
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 275 °F
Middle Barrel Temperature 275 - 300 °F
Front Barrel Temperature 300 - 320 °F
Nozzle Temperature 300 - 330 °F
Melt Temperature 300 - 330 °F
Mold Temperature 80.0 - 120 °F
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0706 / 237197

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.