System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Petropol Nypol® B3 ST PRTA010 NT392 Nylon 6, Impact Modifier, Conditioned
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Impact Grade
Material Notes:
Product Description: Impact Modified, Polyamide 6
Resin ID (ISO 1043): PA6
Additive: High Impact
Processing: Injection Molding
Color: Black
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.04
-
1.08
g/cc
0.0376
-
0.0390
lb/in³
ASTM D792
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
29.0
MPa
4210
psi
ASTM D638
Elongation at Yield
30 %
30 %
ASTM D638
Tensile Modulus
0.540
GPa
78.3
ksi
ASTM D638
Flexural Modulus
0.570
GPa
82.7
ksi
ASTM D790
Izod Impact, Notched
11.89
J/cm
22.27
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Melting Point
215
°C
419
°F
ASTM D2117
Processing Properties
Metric
English
Comments
Processing Temperature
240
-
270
°C
464
-
518
°F
Molding
Mold Temperature
60.0
-
90.0
°C
140
-
194
°F
Drying Temperature
100
°C
212
°F
Dry Time
3.00
hour
3.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PPETROPOL205 / 313113
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.