MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SisiB Silicones FSE9250 Fluoro Silicone Rubber
Categories: Polymer; Thermoset; Silicone

Material Notes: Benefit:
  • Superior extreme (low-high) temperature performance
  • It has very good oil, fuel and liquid resistance.
  • It is useable for molding, extrusion and calendering processes.
  • Typical applications include aerospace fuel system components, diaphragms, gaskets, hose lining, seals and O-rings.

Information provided by SiSiB Silicones - PCC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050
 42
@Temperature 23.0 °C,
Time 252000 sec
42
@Temperature 73.4 °F,
Time 70.0 hour
Oil resistance
 53
@Temperature 230 °C,
Time 252000 sec
53
@Temperature 446 °F,
Time 70.0 hour
Heat Resistance
Tensile Strength 4.46 MPa647 psiOil resistance
 7.38 MPa1070 psiHeat Resistance
 9.50 MPa1380 psi
Elongation at Break 224.4 %224.4 %Heat Resistance
 380 %380 %
Resilience 3232
Tear Strength >= 20.0 kN/m>= 114 pliCrescent
Compression Set 11 %
@Temperature 180 °C,
Time 79200 sec
11 %
@Temperature 356 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Shrinkage 23 %
@Temperature 23.0 °C,
Time 252000 sec
23 %
@Temperature 73.4 °F,
Time 70.0 hour
Volume change, Oil resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSISIB149 / 318808

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.