MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: 40% glass fiber, high melt flow for injection molding

AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK)designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemical resistance expected of PEEK while maintaining excellent elevated temperature properties.

The price and performance of this resin will expand the opportunities for PEEK resins especially in the area of metal replacement for corrosion control.

- Natural: AvaSpire® AV-750 GF40 NT

Markets/Uses: Aircraft / Mechanical & Structural Applications / Electrical Connectors; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping

Applications: Aircraft Applications; Electrical/Electronic Applications; Metal Replacement; Seals

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 450 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ASTM D785
Tensile Strength 191 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 188 MPa
@Thickness 5.00 mm
Type 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.8 %5.0 mm/min; ASTM D638
 1.8 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 15100 MPa5.0 mm/min; ASTM D638
 16700 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 250 MPaISO 178
 54.0 MPa
@Temperature 250 °C
ASTM D790
 253 MPa
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 14800 MPaASTM D790
 15400 MPaISO 178
Compressive Strength 182 MPaASTM D695
Shear Strength 89.0 MPaASTM D732
Izod Impact, Notched 53.0 J/mASTM D256
Izod Impact, Unnotched 590 J/mASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 41.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+17 ohm-cmASTM D257
Surface Resistance >= 1.90e+17 ohmASTM D257
Dielectric Constant 3.66
@Frequency 1e+6 Hz
ASTM D150
 3.68
@Frequency 60 Hz
ASTM D150
 3.69
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.0 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0020
@Frequency 60 Hz
ASTM D150
 0.0030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Specific Heat Capacity 1.26 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.62 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.310 W/m-KASTM C177
Melting Point 345 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 285 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 150 °CDSC
Flammability, UL94 V-1
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 370 - 395 °CInjection
Mold Temperature 175 - 210 °C
Drying Temperature 150 - 175 °C
@Time 9000 - 14400 sec
Back Pressure 0.138 - 0.345 MPa
Screw Speed 75 rpm
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4158 / 279958

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.