MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C34900
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Fair to excellent corrosion resistance. Good cold workability, fair hot workability for bending and forming, heading and upsetting, machining, roll threading and knurling.

Applications: building hardware, rivets and nuts, plumbing goods and parts, requiring moderate cold working combined with some machining.

Available as rod and wire.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.44 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 365 - 469 MPa
Tensile Strength, Yield 110 - 379 MPaDepending on temper
Elongation at Break 72 %in 457.2 mm.
Modulus of Elasticity 105 GPa
Poissons Ratio 0.35Calculated
Machinability 50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 895 - 910 °C
Solidus 895 °C
Liquidus 910 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 61 - 64 %
Iron, Fe <= 0.10 %
Lead, Pb 0.10 - 0.50 %
Other, total <= 0.50 %
Zinc, Zn 37.45 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Tin-Bearing Copper Nickel, UNS C72500, Quarter Hard flat products
Copper, UNS C40800
Copper, UNS C41300
Forging Brass, UNS C37700

MC34900b1 / 11212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.