MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear® 22 Quench Oil
Categories: Fluid; Quenchant

Material Notes: Description: Conoco Hydroclear® Quench Oil is a high-quality metal heat-treating and quenching oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Quench Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of quenching, spraying and heat-treating applications where controlled cooling rates are required. Hydroclear Quench Oil provides exceptional oxidation stability, good rust and corrosion protection, excellent filterability and uniform cooling of metal parts. Hydroclear Quench Oil is available in ISO viscosity grades 22 and 32HS. Hydroclear Quench Oil 32HS is formulated with special quench improvers for applications which require higher quenching speeds.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.16 lb/gal
Viscosity Measurement 96Viscosity Index
Saybolt Viscosity at 100°F 125 SUS
Saybolt Viscosity at 210°F 41 SUS
Kinematic Viscosity at 40°C (104°F) 22 cSt
Kinematic Viscosity at 100°C (212°F) 4.5 cSt
ASTM Color 0.00
 
Thermal PropertiesOriginal ValueComments
Pour Point 9.00 °F
Flash Point 425 °F
 
Descriptive Properties
Quench Time16 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ConocoPhillips Hydroclear® AW 22 Hydraulic Fluid
Phillips 66 Quench Oils 32HS ISO Grade 32
Phillips 66 Quench Oils 22 ISO Grade 22
ConocoPhillips Hydroclear® 32HS Quench Oil
ChevronTexaco Quenchtex® A

WCON109 / 75146

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.