MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Fireguard® 910-FOB-NL1 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Uses: Plenum Cable Jacketing; Wire and Cable Applications

Agency Ratings: UL QMTT2 .E200337

Forms: Pellets

Additional Information:

Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes to Decomposition): 57

Kayness ACR at 350°F, 1000 sec-1: 290 Pa-s

Cone Calorimeter at 75 kW/m2, Peak Heat Release Rate: 111 kW/m2

Average Heat Release Rate: 60 kW/m2

Total Heat Released: 77 MJ/m2

Average Heat of Combustion: 13.5 MJ/kg

Average Specification Extinction Area: 325 m2/kg

Peak Smoke: 2.3 1/m

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore C 838310 seconds; ASTM D2240
Tensile Strength at Break 17.2 MPa2500 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.59
@Frequency 1e+6 Hz
3.59
@Frequency 1e+6 Hz
ASTM D150
 4.65
@Frequency 1000 Hz
4.65
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 30.3 kV/mm770 kV/inASTM D149
Dissipation Factor  0.035
@Frequency 1e+6 Hz
0.035
@Frequency 1e+6 Hz
ASTM D150
 0.083
@Frequency 1000 Hz
0.083
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 75.0 °C167 °FContinuous Use; ASTM D794
Brittleness Temperature -8.00 °C17.6 °FASTM D746
Oxygen Index 42 %42 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Fireguard® 910-A10-NL2 Polyvinyl Chloride, Flexible
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Teknor Apex Fireguard® 910-NL1 Polyvinyl Chloride, Flexible
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 29 Aramid Fiber

PTEKNO602 / 128780

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.