MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Osterman & Co Osterlene® LLB200-B LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LLB200 features a low gel level and exhibits excellent toughness and strength when drawn down to thing gauges in blown and cast film applications. Use for LLB200 include, bags – heavy duty bags, industrial applications, packaging cast, liners, stretch wrap and film.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America
Additive: Antiblock: No; Slip: No
Features: Butene Comonomer; High Strength; High Toughness; Low Gel
Uses: Bags; Blown Film; Cast Film; Film; Heavy-duty Bags; Industrial Applications; Liners; Packaging; Stretch Wrap
Processing Method: Blown Film; Cast Film; Extrusion

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 650 %650 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Secant Modulus, MD 0.193 GPa28.0 ksiASTM D790
Secant Modulus, TD 0.207 GPa30.0 ksiASTM D790
Elmendorf Tear Strength MD 120 g120 gASTM D1922
Elmendorf Tear Strength TD 400 g400 gASTM D1922
Dart Drop Test 100 g0.221 lbASTM D1709
Film Tensile Strength at Break, MD 28.3 MPa4100 psiASTM D882
Film Tensile Strength at Break, TD 24.1 MPa3500 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 15 %15 %ASTM D1003
Gloss 50 %50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER095 / 267677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.