The listed composition is for semifinished products for forging, hot-rolled and cold-finished bars, wire rods and seamless tubing. This alloy was formerly known as SAE 1048 before SAE adopted the AISI 1548 designation. |
UNS G15480, ASTM A29, ASTM A510, ASTM A576, SAE J403, SAE J412, SAE J414, DIN 1.1226 |