MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Barlog Plastics KEBALLOY ECO R-PET E401 100% PET recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: KEBALLOY ECO R-PET E401 is a recycled, medium viscosity PET grade (polyethylene terephthalate) approved for direct food applications. The material is supplied as crystallized granules. This grade is produced from 100% post-consumer bottle flakes.

Properties: amorphous, dimensionally stable, compliant for food contact (according to 10/2011 EC), semi-crystalline, approved for food contact (EU and FDA)

Typical areas of application: Glasses frames, Cover, Filter cups, Housing, Crockery and cutlery, industrial goods, Cosmetic packaging, Food packaging, Toys, Sports & Leisure Articles

Industries: Household appliances, Industry, Agriculture, Food processing industry, Sanitary industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaISO 527-1
Elongation at Yield 4.00 %ISO 527-1
Modulus of Elasticity 2.50 GPaISO 527-1
Charpy Impact Unnotched 260 kJ/m²ISO 179-1eU
Charpy Impact, Notched 3.50 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 247 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CISO 75-1/-2
Vicat Softening Point 74.0 °C50°C/h, 50N; DIN EN ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 290 °Chot runner
Melt Temperature 270 - 300 °C
Mold Temperature <= 20.0 °C
Drying Temperature 160 °C
Dry Time 4.00 - 6.00 hour
Moisture Content <= 0.00500 %
Back Pressure 4.00 - 8.00 MPa
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBARLO669 / 326743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.