MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, Frameworks of Deflection Coils, Hi-Pressure Outputs Package, Plugs of Kinescopes Autos and Others: Ignition Systems, Heating Systems, Electricity Distribution Systems, Tail Lights Base, Shells of Ignition Coils, Door Handles, Air-Condition Lattices

Information provided by Zhejiang Juner New Materials Co, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccD792
Water Absorption 0.090 %23°C•24h; D570
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cmD955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 115 MPaD638
Elongation at Break 4.0 %D638
Flexural Strength 180 MPaD790
Flexural Modulus 8.00 GPaD790
Charpy Impact Unnotched 4.80 J/cm²IS0179
Charpy Impact, Notched 1.00 J/cm²IS0179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmD257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
D150
Dielectric Strength 21.0 kV/mmD149
Dissipation Factor 0.025
@Frequency 1e+6 Hz
D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
D696
Deflection Temperature at 1.8 MPa (264 psi) 205 °CD648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 255 - 265 °C
Nozzle Temperature 245 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 130 - 140 °C
@Time 14400 sec
Injection Pressure 80.0 - 120 MPa3-15 sec
Back Pressure 8.00 - 18.0 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
LG Chemical HI100H ABS, High Impact, High Toughness
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
Zhejiang Juner 201-G20 20% Glass Fibre Reinforced

PJUNER56 / 48569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.