MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax PC Series™ PC Max™ Paper Ceramic Fiber Filtration Media
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: PC (Porosity Controlled) Series™ Papers perform the following critical functions in all types of pyrotechnic automotive airbag inflator filters: (1) Provide efficient filtration of effluent gas by removing particulate matter through condensation and adhesion and mechanical entrapment. (2) Through the removal of high heat capacity particulate matter, these aluminosilicate filtration media significantly cool the gas stream before it enters the bag. (3) Consistently regulate gas flow into the bag ensuring conformance to the planned deployment sequence.

PC Max™ are filtration media formulated from high alumina chemistry fiber and developed for specific applications requiring temperature capability above that provided by typical ceramic fiber chemistries.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition <= 8.0 %
 
Component Elements PropertiesOriginal ValueComments
Al2O3 97 %
SiO2 2.0 %
 
Descriptive Properties
Basis Weight (lb/3000ft2)425
Caliper (in.)0.165at 8 PSF
 0.3at 4 PSF
Other (%)1
Resistance (mm H2O)30at 85 l/min/100cm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR CIMBAR™ PC Barite Powder (BaSO4)
Unifrax PC Series™ 200 Paper Ceramic Fiber Filtration Media
3M Nextel™ 650 Composite Ceramic Fiber
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Pyrotek Grade 1250 Ceramic fiber paper

CUNIF133 / 97905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.