MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
Eastman Eastar™ 6763 Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Meets ISO 10993 and/or USP Class VI biocompatibility requirement; Food Contact Status compliant. Eastar™ Co polyester 6763 is a clear, amorphous material that can be molded and extruded with ease. Its excellent performance properties include clarity, toughness, good melt strength, no dusting, no stress whitening, good heat sealability, easy cutting and thermoforming. Eastar™ Copolyester 6763 may be colored using color concentrates, dry colors, or liquid colorants. Eastar™ Copolyester 6763 can be safely sterilized with proper ethylene oxide, radiation, or electron beam methods without property loss or color shift. It is well suited for a variety of applications including, medical packaging, cosmetics and personal care packaging, food and beverage packaging, and display & signs.

Application/Uses:

  • Blister packaging
  • Blood Contact
  • Blown film
  • Credit cards
  • Debit cards
  • Deodorant packaging
  • Device Packaging
  • Drug Delivery
  • Electronic packaging
  • Fabricated Boxes
  • Flexible packaging
  • Food packaging
  • Furniture/Furniture trim
  • Gaming cards
  • Gift cards
  • Identification cards
  • IV Components
  • IV Containers
  • Labware
  • Laminating
  • Phone cards
  • Plastic Cards
  • Rigid Medical Packaging
  • Shrink film
  • Signs
  • Smart cards
  • Suction & Drainage
  • Toys/Sporting goods
  • Tubing
  • Writing instruments
Key Attributes:
  • Easy primary & secondary operations
  • Excellent clarity
  • Excellent toughness
  • Gamma, ebeam, ETO sterilization stable

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D1505
 1.27 g/ccInjection Molded; ASTM D792
Water Absorption 0.13 %
@Time 86400 sec
Immersion; ASTM D570
Water Vapor Transmission 91.0 g/m²/day
@Temperature 38.0 °C
100% RH; ASTM F1249
Oxygen Transmission 10.0 cc-mm/m²-24hr-atmASTM D3985
Carbon Dioxide Transmission 49.0 cc-mm/m²-24hr-atmASTM D1434
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 106ASTM D785
 109ISO 2039-2
Tensile Strength at Break 28.0 MPaASTM D638
 28.0 MPaISO 527
Film Tensile Strength at Yield, MD 52.0 MPaASTM D882
Film Tensile Strength at Yield, TD 52.0 MPaASTM D882
Tensile Strength, Yield 50.0 MPaASTM D638
 50.0 MPaISO 527
Film Elongation at Break, MD 400 %ASTM D882
Film Elongation at Break, TD 400 %ASTM D882
Film Elongation at Yield, MD 4.0 %ASTM D882
Film Elongation at Yield, TD 4.0 %ASTM D882
Elongation at Break 100 %ISO 527
 130 %ASTM D638
Tensile Modulus 1900 MPaMD; ASTM D882
 1900 MPaTD; ASTM D882
 2100 MPaASTM D638
 2100 MPaISO 527
Flexural Strength 68.0 MPaISO 178
 70.0 MPaASTM D790
Flexural Modulus 2000 MPaISO 178
 2100 MPaASTM D790
Izod Impact, Notched 37.0 J/m
@Temperature -40.0 °C
ASTM D256
 101 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature -40.0 °C
ASTM D4812
 NB
@Temperature -30.0 °C
ASTM D4812
 NB
@Temperature -20.0 °C
ASTM D4812
 NB
@Temperature 23.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 4.20 kJ/m²
@Temperature -40.0 °C
Type 1 Specimen, Type A Notch; ISO 180
 6.20 kJ/m²
@Temperature 23.0 °C
Type 1 Specimen, Type A Notch; ISO 180
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
Type 1 Specimen; ISO 180
 NB
@Temperature -20.0 °C
Type 1 Specimen; ISO 180
 NB
@Temperature -30.0 °C
Type 1 Specimen; ISO 180
 NB
@Temperature -40.0 °C
Type 1 Specimen; ISO 180
Puncture Energy 28.0 J
@Temperature 23.0 °C
Energy @ Max. Load, 2.5-mm Thick Plaques; ASTM D3763
 33.0 J
@Temperature 23.0 °C
Energy @ Max. Load, 3.2-mm Thick Plaques; ASTM D3763
 35.0 J
@Temperature -40.0 °C
Energy @ Max. Load, 2.5-mm Thick Plaques; ISO 6603-2
 36.0 J
@Temperature -40.0 °C
Energy @ Max. Load, 3.2-mm Thick Plaques; ISO 6603-2
 40.0 J
@Temperature 23.0 °C
Energy @ Max. Load, 2.5-mm Thick Plaques; ISO 6603-2
 41.0 J
@Temperature -40.0 °C
Energy @ Max. Load, 2.5-mm Thick Plaques; ASTM D3763
 44.0 J
@Temperature 23.0 °C
Energy @ Max. Load, 3.2-mm Thick Plaques; ISO 6603-2
 50.0 J
@Temperature -40.0 °C
Energy @ Max. Load, 3.2-mm Thick Plaques; ASTM D3763
Tear Strength, Total 93.0 NMD, PPT; ASTM D2582
 93.0 NTD, PPT; ASTM D2582
Tear Strength 36.0 kN/mMD, Propagation Resistance, Split Tear Method, 254 mm/min; ASTM D1938
 36.0 kN/mTD, Propagation Resistance, Split Tear Method, 254 mm/min; ASTM D1938
 36.0 kN/mMD, Trouser @ 200 mm/min; ISO 6383-1
 36.0 kN/mTD, Trouser @ 200 mm/min; ISO 6383-1
Elmendorf Tear Strength MD 1400 gASTM D1922
Elmendorf Tear Strength TD 1700 gASTM D1922
Dart Drop Test 400 g
@Temperature 23.0 °C
ASTM D1709A Modified
 500 g
@Temperature -18.0 °C
ASTM D1709A Modified
Film Tensile Strength at Break, MD 59.0 MPaASTM D882
Film Tensile Strength at Break, TD 55.0 MPaASTM D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 2.4
@Frequency 1e+6 Hz
ASTM D150
 2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm500 V/sec rate-of-rise; ASTM D149
Dissipation Factor 0.0050
@Frequency 1000 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 158 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 51.0 µm/m-°C
@Temperature -30.0 - 40.0 °C
ASTM D696
Specific Heat Capacity 1.30 J/g-°C
@Temperature 60.0 °C
 1.76 J/g-°C
@Temperature 100 °C
 1.88 J/g-°C
@Temperature 150 °C
 1.97 J/g-°C
@Temperature 200 °C
 2.05 J/g-°C
@Temperature 250 °C
Thermal Conductivity 0.210 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CASTM D648
Vicat Softening Point 85.0 °CASTM D1525
Glass Transition Temp, Tg 80.0 °C
 
Optical PropertiesOriginal ValueComments
Haze 0.80 %ASTM D1003
Gloss 108 %45°; ASTM D2457
Transmission, Visible 89 %Regular; ASTM D1003
 91 %Total; ASTM D1003
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm CYROLITE G20-HIFLO Acrylic-Based Multipolymer Compound
Eastman Eastar 6763 PETG Copolyester
Eastman Eastar MN211 Copolyester, Natural
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness

PEATM5111 / 222305

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.