MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® LVX-50H black 9230 PA12-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are:
  • Very high stiffness and strength
  • Excellent impact and notched impact strength
  • Excellent UV, heat and chemical resistance
  • Very low moisture absorption
  • Suitable for repeated steam sterilization
  • Good flow characteristics
  • High molding precision, low warpage
Grilamid LVX-50H black 9230 is especially suitable for complex structural parts in applications such as:
  • Electronic devices
  • Automotive
  • Mechanical engineering
  • Safety components
  • Medical devices and instruments
  • Sports & leisure goods

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccDry; ISO 1183
Water Absorption 0.80 %Sim. to ISO 62
Moisture Absorption 0.400 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaConditioned; ISO 527-1/-2
Elongation at Break 3.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 12000 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 85.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 20.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 55.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 175 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 130 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Compressed air systems
 Exterior
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Lighting
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesImproved flowability and demolding
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® L 20 EC PA12-CD25
Avient PolyOne® ND-10 Ethylene-Propylene Diene Elastomer (EPDM) Compound
EMS-Grivory Grilamid® LV-3 X ESD black PA12-GF30
EMS-Grivory Grilamid® LV-30H FWA nat PA12-GF30
EMS-Grivory Grilamid® LVX-50H nat PA12-GF50

PGRH090 / 156799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.