MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MAS Epoxies DEEP POUR Two-component epoxy system 100% solids
Categories: Polymer; Thermoset; Epoxy

Material Notes: The MAS Deep Pour Epoxy Resin System is a 100% solids, two-component, three to one by volume room temperature curing epoxy resin system formulated for deep pour casting, encapsulating and molding applications. It cures to a clear, glass-like finish that resists scratching and yellowing with an extended gel time to minimize exotherm and improve air release. Epoxy system specifically designed for casting, Clear system is compatible with a variety of colorants if desired, Long gel time to mitigate yellowing and cracking during cure.

Information provided by MAS Epoxies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.947 g/cc0.0342 lb/in³Hardener; ASTM D1475
 1.15 g/cc0.0415 lb/in³Cured; ASTM D792
Viscosity 10 cP10 cPHardener; ASTM D2196
 260 cP260 cPInitial Mixed; ASTM D2196
 1000 cP1000 cPResin; ASTM D2196
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
Tensile Strength 55.8 MPa8100 psiASTM D638
Elongation at Break 4.3 %4.3 %ASTM D638
Flexural Strength 92.94 MPa13480 psiASTM D790
Flexural Modulus 3.02282 GPa438.423 ksiASTM D790
Compressive Strength 77.63 MPa11260 psiASTM D695
Izod Impact, Notched 0.448 J/cm0.840 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 47.8 °C118 °FHDT load unknown, room temp cure; ASTM D648
 50.0 °C122 °FHDT load unknown, post cure; ASTM D648
Shrinkage 3.85 %3.85 %ASTM D792/2196 (volumetric)
 
Processing PropertiesMetricEnglishComments
Gel Time 330 min330 min150g mass; ASTM D2471
 
Descriptive Properties
ColorClear
Mix Ratio by Volume3A : 1B
Mix Ratio by Weight100A : 28B
Volumetric Yield (in³/lb)25ASTM D792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASZ902 / 265517

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.