MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound DX11355 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DX11355 compound is based on Polycarbonate (PC) resin containing proprietary fillers and available in black color only. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Improved Impact, Non-Brominated, Non-Chlorinated Flame Retardant.

Features: Enhanced Ductility,Laser Direct Structuring,Flame Retardant,Circuit Solution,Colorable,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
Moisture Absorption 0.0100 %0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
12 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.0 MPa7540 psi50 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa8410 psi50 mm/min; ASTM D638
Elongation at Break 70 %70 %50 mm/min; ASTM D638
Elongation at Yield 5.4 %5.4 %50 mm/min; ASTM D638
Tensile Modulus 2.60 GPa377 ksi50 mm/min; ASTM D638
Flexural Strength 89.0 MPa12900 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 90.0 MPa13100 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.40 GPa348 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 800 J590 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.92
@Frequency 1e+9 Hz
2.92
@Frequency 1e+9 Hz
IEC 60250
Dissipation Factor 0.0070
@Frequency 1e+9 Hz
0.0070
@Frequency 1e+9 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 62.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
34.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
@Thickness 3.20 mm
237 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.600 mm
V-0
@Thickness >=0.0236 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 300 °C527 - 572 °F
Zone 2 255 - 295 °C491 - 563 °F
Zone 3 260 - 300 °C500 - 572 °F
Melt Temperature 275 - 300 °C527 - 572 °FInjection Molding
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 100 - 110 °C212 - 230 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 80 %30 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81562 / 289509

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.