MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Avient Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant® compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0070 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 43.4 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 100 %Type I, 51 mm/min; ASTM D638
Flexural Strength 59.3 MPaASTM D790
Flexural Modulus 1790 MPaASTM D790
Izod Impact, Notched 690 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 249 - 271 °C
Deflection Temperature at 0.46 MPa (66 psi) >= 80.0 °C
@Thickness 3.18 mm
Annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Mold Temperature 37.8 - 60.0 °C
Drying Temperature 82.2 °C
Dry Time 3.00 hour
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
AppearanceNatural Color
FeaturesBiocompatible
 Good Chemical Resistance
 Good Colorability
 High Impact Resistance
 Specialty Grade
FormsPellets
Generic MaterialPC+PBT
Generic NamePolycarbonate + PBT (PC+PBT)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesHospital Goods
 Housings
 Medical Appliances
 Medical/Healthcare Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT)
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Kingfa LONOY 2100 LT PC/PET Alloy
A. Schulman Diamond DIAMALOY 530 PC/PBT Alloy, UV Stabilized/Weatherable
A. Schulman Diamond DIAMALOY 527 PC/PBT Alloy

PH0POL1250 / 145819

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.