MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service temperature range of -60°F to 400°F. Other salient characteristics include dimensional stability, outstanding physical strength and good flowability. This latter property enables it to be readily used for potting and encapsulation applications. EP30ANHT is also brushable and can be used as an adhesive, coating and sealant. In this regard, it bonds well to metals, many plastics, ceramics and glass. It resists a variety of chemicals including water, oils, fuels, acids and bases. EP30ANHT has a very low coefficient of thermal expansion (CTE). It is formulated to cure at room temperature or more rapidly at elevated temperatures and has a ten to one (10:1) mix ratio by weight. The color of Part A is gray and Part B is clear. Master Bond EP30ANHT is widely used in the electronic, electrical, computer, chemical, electro-optical and related industries where maximum heat transfer and superior electrical isolation are required.

Product Advantages:

  • Easy application: adhesive spreads or pours evenly and smoothly.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures.
  • High bond strength to a wide variety of substrates; very good adhesive properties.
  • Accomplished electrical insulator with impressively high capacity for heat transfer.
  • Great dimensional stability, high compressive strength and low CTE.
  • Low viscosity with excellent flowability; ideal for potting and encapsulation.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 280 - 500 cP280 - 500 cPPart B
 60000 - 110000 cP60000 - 110000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Tensile Strength at Break >= 41.4 MPa>= 6000 psi
Compressive Strength >= 117 MPa>= 17000 psi
Shear Strength >= 6.21 MPa>= 900 psiTensile, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Constant 4.6
@Frequency 60 Hz,
Temperature 25.0 °C
4.6
@Frequency 60 Hz,
Temperature 77.0 °F
Dielectric Strength >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.0 - 25.0 µm/m-°C12.2 - 13.9 µin/in-°F
Thermal Conductivity 3.17 - 3.60 W/m-K22.0 - 25.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 93.3 °C
1.00 - 2.00 hour
@Temperature 200 °F
 1440 - 2880 min
@Temperature 23.9 °C
24.0 - 48.0 hour
@Temperature 75.0 °F
Pot Life 40 - 60 min40 - 60 min100 gram batch
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened container
 
Descriptive Properties
Mixing Ratio (A to B)10:1by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow TC-5688 Thermally Conductive Compound
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond EP42HT-2AN Thermally Conductive Potting Compound
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting

PMASTB371 / 149618

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.